Brand Name : DINGSCO
Model Number : According to customers' requests
Certification : ISO 9001:2015, PED 2014/68 EU, API 6A, API-20B, TSG, NORSOK
Place of Origin : China
MOQ : Negotiable
Price : Negotiable
Payment Terms : T/T
Supply Ability : Negotiable
Delivery Time : (Sample order) 7 days
Packaging Details : According to customers' requests
Product Name : Hastelloy X Valve Gate
Alloy Type : Nickel-based superalloy
Spec. : As required
Pressure : 15-140Mpa
Chemical Composition : Balance Ni, 21%Cr, 19%Fe...
Features : Corrosion Resistant
Hastelloy X Valve Gate For Petroleum Equipment Valve Plate
Valve gate is a gate system component used in the plastic injection molding process. Its main function is to control the flow of plastic melt during the plastic injection molding process in order to better control the quality of plastic products and reduce waste. Valve gate systems typically consist of one or more controllable on/off valves that precisely control the rate and amount of melt flowing into the mold.
Compared with other gate systems (such as hot runner systems), valve gate systems have higher flexibility and control capabilities, and are suitable for injection molding applications that require higher product quality.
| Grade | UNS | density | GB | ||||
| Hastelloy X | N06002 | 8.22g/cm³ | GH3536 | ||||
| Chemical Composition(%) | Ni | Cr | Fe | C | Mn | S | Si |
| Remainder | 0.05-0.15 | 17.0-20.0 | 0.05-0.15 | 1.0max | 0.03max | 1.0max | |
| Mo | P | Co | S | W | |||
| 8.0-10.0 | 0.04max | 0.5-2.5 | 0.03max | 0.20-1.0 | |||
| Physical Properties | Tensile Strength ( Mpa min) | Yield Strength ( Mpa min) | Reduction of Area ,min (%) | Elongation min(%) | Hardness (HRC) | ||
| 660 MPa min | 240 MPa min | …. | 35% min | … | |||
Hunan Dinghan New Material Technology Co., Ltd. (DINGSCO) specialized in Nickel Based Corrosion Resistant and High Temperature alloys products which used in the world’s most technically demanding industries and applications.We are dedicated to providing our customers with best quality products, fastest possible deliveries, most competitive prices of Nickel Based Corrosion Resistant and High Temperature alloys in bars, rods, forged flanges, valve parts (Ball, Stem, Seat Ring, etc), forged shapes (shafts, discs, blocks, hubs, rings, cylinders and other custom shapes) according to ASTM, ASME, API, AMS, NACE and other industry standards.

PROFESSIONAL NICKEL ALLOY MANUFACTURER
CORE VALUE
CUSTOMIZED PRODUCTS:

APPLICATION:

|
|
Hastelloy X Valve Gate / Nickel Based Superalloy Valve Plate For Petroleum Equipment Images |